Chemical porcelain has an average coefficient of expansion from 20°C to 200°C is 3.56 x 10-6, gradually increasing to 4.69 x 10-6 at 1000°C. Note: To prevent thermal stress cracks on porcelain ware it is strongly recommended a heating/cooling rate not to exceed 200°C/hour. There are small perforations throughout this desiccator plate, and one large hole in center. The plate is glazed on one side and is without feet.
Specification
Hole diam.: 2 mm, small; 23 mm, center Plate diam.: 230 mm
Refractory Qualities Fusion point: 1670°C Softening point: 1400°C Limit of use, unglazed: 1400°C Limit of use, glazed: 1150°C Limit of use, evacuated: 1300°C
Related Products
Porcelain Desiccator Plates, Small Perforations, Plate Diam. 190 mm, Coorstek (CAT#: STEM-GLE-0728-LKN) Porcelain Desiccator Plate, Plate Diam. 190 mm, No. of Holes, 7, Coorstek (CAT#: STEM-GLE-0730-LKN) Porcelain Desiccator Plate, Plate Diam. 95 mm, No. of Holes, 3, Coorstek (CAT#: STEM-GLE-0731-LKN) Porcelain Desiccator Plate, Plate Diam. 230 mm, No. of Holes, 8, Coorstek (CAT#: STEM-GLE-0732-LKN) Porcelain Desiccator Plate, Plate Diam. 142 mm, No. of Holes, 5, Coorstek (CAT#: STEM-GLE-0733-LKN)